A COMPARATIVE ANALYSIS OF CONCRETE STRENGTH USING IGNEOUS, SEDIMENTARY
The 28-day concrete cubes cast with these aggregates shows that, at the low strength of 20 N/mm2, igneous rock - crushed granite stone c concrete had the highest strength of 26.45 N/mm2 followed by Sedimentary-limestone with 26.11 N/mm2 and metamorphic rock - marble stone 26.03 N/mm2 in that order, and also at the high strength of 30 N/mm2 ...